Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 2 micron Microslit SKU: MSSN400.C-3LX.1-2.0K2 Lot Number: 250409-07 Quantity Received: 170 Notes: Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 3.64 2psi: 5.49 4psi: 8.18 15psi: 17.52 Burst: 59.17 PSI…