Discoloration Study with Bacterial Media

I performed a test study to see the effect of microbial media’s : LB and BHI Broth on the membrane to check for discoloration. LB Broth : Lysogeny broth,Luria broth or Luria-Bertani broth. Obtained from Sigma and made by dissolving…