Tag: nakul

Vacuole formation on Nitride

Barrett had discovered that growing endothelial cells on pnc-si or tranwells causes vacuoles to form. The vacuoles on pnc-si formed only on the free standing areas of the membrane where there are open pores. The background on pnc-si chips showed…

Posted in NRG Tagged with: , ,

Discoloration CVC vs. AJA Tool

Based on Barrett’s array set up for discoloration, I set up an array experiment to check the discoloration effects between the new and old system ( 2e-7,AJA vs the older 7e-7 CVC ). The wafers from each had a bit…

Posted in NRG Tagged with: , , ,

Discoloration Study with Bacterial Media

I performed a test study to see the effect of microbial media’s : LB and BHI Broth on the membrane to check for discoloration. LB Broth : Lysogeny broth,Luria broth or Luria-Bertani broth. Obtained from Sigma and made by dissolving…