Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 8 micron Microslit – Gold Coated SKU: MSSN400.C-3LX.1-8.0K2-AU Lot Number: 251028-10 Quantity Received: 200 Manufacturer Test Report: Flow Data Avg in SLPM 15psi: 7.6 Burst: 16.1 PSI
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 8 micron Microslit – Gold Coated SKU: MSSN400.C-3LX.1-8.0K2-AU Lot Number: 251028-10 Quantity Received: 200 Manufacturer Test Report: Flow Data Avg in SLPM 15psi: 7.6 Burst: 16.1 PSI
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 0.5 micron Microslit SKU: MSSN400.C-3LX.1-0.5E1 Lot Number: 250409-13 Quantity Received: 250 Manufacturer Test Report: Flow Data Avg in SLPM 4psi: 3.96 15psi: 14.4 Burst: 9.82 PSI
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 0.5 micron Microslit SKU: MSSN400.C-3LX.1-0.5E1 Lot Number: 251028-02 Quantity Received: 250 Manufacturer Test Report: Flow Data Avg in SLPM 4psi: 3.88 15psi: N/A Burst: 9.22 PSI
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250413-11 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 43.2 nm Porosity: 10.3% Flow Data Avg in SLPM 2psi: 0.06 4psi: 0.13 Burst: 6.7…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250413-12 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 44.9 nm Porosity: 9.8% Flow Data Avg in SLPM 2psi: 0.06 4psi: 0.12 Burst: 7.43…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250413-14 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 48.4 nm Porosity: 10.8% Flow Data Avg in SLPM 2psi: 0.06 4psi: 0.12 Burst: 7.98…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 250413-13 Quantity Received: 250 Notes: Manufacturer Test Report: Pore Size: 44.8 nm Porosity: 9.8% Flow Data Avg in SLPM 2psi: 0.06 4psi: 0.12 Burst: 7.32…
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: Non Porous SKU: SN400.C-3X.1 Lot Number: 2510022-13 Quantity Received: 250 Notes: UR Testing For more information visit:
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: Non Porous SKU: SN400.C-3X.1 Lot Number: 240913-22 Quantity Received: 250 Notes: UR Testing For more information visit:
Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 2 micron Microslit SKU: MSSN400.C-3LX.1-2.0K2 Lot Number: 250409-09 Quantity Received: 330 Notes: extra 100 in air filter disks Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 3.97 2psi: 5.61 4psi:…