Wafer #250409-07 – 2 μm Microslit

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 2 micron Microslit SKU: MSSN400.C-3LX.1-2.0K2 Lot Number: 250409-07 Quantity Received: 170 Notes: Manufacturer Test Report: Flow Data Avg in SLPM 1psi: 3.64 2psi: 5.49 4psi: 8.18 15psi: 17.52 Burst: 59.17 PSI…

Posted in Wafer QC Pages

Wafer #250409-11 – 4 μm Microslit

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 4 micron Microslit SKU: MSSN400.C-3LX.1-4.0K2 Lot Number: 250409-11 Quantity Received: Notes: Manufacturer Test Report: Flow Data Avg in SLPM 4psi: 8.26 15psi: 17.24 Burst: 36.86 PSI UR Testing Porosity: Pore size:…

Posted in Wafer QC Pages

Wafer #250409-10 – 4 μm Microslit

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: MSSN 4 micron Microslit SKU: MSSN400.C-3LX.1-4.0K2 Lot Number: 250409-10 Quantity Received: Notes: Manufacturer Test Report: Flow Data Avg in SLPM 2psi: 5.63 4psi: 8.1 15psi: 16.96 Burst: 37.35 PSI UR Testing Porosity:…

Posted in Wafer QC Pages

Wafer #240914-19 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-19 Quantity Received: Manufacturer Test Report: Pore Size: 64.1 nm Porosity: 21.5% Flow Data Avg in SLPM 1psi: 0.12 2psi: 0.23 Burst: 3.66 PSI UR…

Posted in Wafer QC Pages

Wafer #240914-20 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-20 Quantity Received: Manufacturer Test Report: Pore Size: 40.3 nm Porosity: 13% Flow Data Avg in SLPM 1psi: 0.13 2psi: 0.26 Burst: 3.04 PSI UR…

Posted in Wafer QC Pages

Wafer #240914-21 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-21 Quantity Received: Manufacturer Test Report: Pore Size: 44.4 nm Porosity: 13.5% Flow Data Avg in SLPM 1psi: 0.12 2psi: 0.25 Burst: 3.49 PSI UR…

Posted in Wafer QC Pages

Wafer #240914-08 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-08 Quantity Received: Manufacturer Test Report: Pore Size: 45.4 nm Porosity: 15.1% Flow Data Avg in SLPM 1psi: 0.235 4psi: 0.343 Burst: 3.521 PSI UR…

Posted in Wafer QC Pages

Wafer #240914-15 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-15 Quantity Received: Manufacturer Test Report: Pore Size: 64 nm Porosity: 20.7% Flow Data Avg in SLPM 1psi: 0.12 2psi: 0.23 Burst: 3.46 PSI UR…

Posted in Wafer QC Pages

Wafer #240914-24 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240914-24 Quantity Received: Manufacturer Test Report: Pore Size: 56.5 nm Porosity: 20.3% Flow Data Avg in SLPM 2psi: 0.107 4psi: 0.201 Burst: 5.962 PSI UR…

Posted in Wafer QC Pages

Wafer #240803-21 – 1 Slot NPN

Manufacturer’s Data Logged by: Ahmet Gurcan Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240803-21 Quantity Received: Manufacturer Test Report: Pore Size: 75.2 nm Porosity: 21.9% Flow Data Avg in SLPM 2psi: 0.177 4psi: 0.363 Burst: 5.48 PSI UR…