Using a 6″ wafer, we start with 50 nm of RV SiN, then deposit 40 nm a-Si followed by 20 nm of SiO2. RTP of 1050 C, 100 C/s, 60s. JP patterned the wafer to make standard SEPCON chips. The…
Using a 6″ wafer, we start with 50 nm of RV SiN, then deposit 40 nm a-Si followed by 20 nm of SiO2. RTP of 1050 C, 100 C/s, 60s. JP patterned the wafer to make standard SEPCON chips. The…
It was decided during my rotation-review meeting to use a smaller PEG molecule (3-mer) for silanization of pncSi. Following is the brief description of the polymer. Boiling Point: 147-9°C @ 0.3mm Freezing…
Previously, I had gotten some inexplicable results showing that increasing salt concentration decreases the flow through a membrane. This makes no sense (and goes against our previous data) because we would expect electrostatic forces to counteract the flow, an effect…
As the device animation shows, the layout of the chip has changed. The incorporation of through-vias in the bulk silicon allows me to eliminate a gasket wrapping around the filter, which was a large source of leaks. I used ozone…
In order to address the fluctuations in the clearance data at the beginning of the long term treatment previous post The new protocol is as follows: 1. An inspected single slot dialysis chip is clamped into an acrylic fixture holding…
BBB Device V2-8 Filling Up by the way, the code to embed .mp4 videos uploaded to the server is: ” <video width=”640″ height=”360″ controls> <source src=”http://example.com/wp-content/uploads/video.mp4″ type=’video/mp4′></source> <source src=”http://example.com/wp-content/uploads/video.ogv” type=’video/ogg’></source> </video>”
How to use the McGrath Lab Surface Contact Angle Goniometer (SCAG) to collect image data for the established uses. Please refer to the SCAG Setup Protocols for assembly instructions. Note that the details of established uses will be covered in a…
How to prepare the McGrath Lab Surface Contact Angle Goniometer (SCAG) from a disassembled form. I will create detailed posts on potential uses in the future. GENERAL NOTES Based on the McGrath Lab SCAG as it was on May 16th, 2013 Instrument…
Although the connection of those electrical circuits was always unstable, Greg and I did get some TEER measurement with this set up: Device A Day 1 Day 2 Day 3 Day 4 Day 5 EVOM 1 -3450Ω* -1000Ω -1200…