Rhodamine transport in transwells

I finished the first experiment to look at rhodamine transport across commercial transwell membranes. I was mainly interested if there would be enough transport into the basolateral chamber to measure the rhodamine with the spec. Experimental details: both chambers in…

Posted in NRG Tagged with: ,

Silanization and Membrane Chemical Stability

Due to our desire to improve membrane stability in cell culture, different methods of treatment have been mentioned to try, including carbonization and silanization. W606 was treated with UV/ozone at 150C for 20 minutes, followed by silanization performed by some…