Tag: NSN

Burst Pressure, Permeance of NSN pnc-Si SEPCONS with large pores

Karl, Charles and I measured the burst pressure and permeance of some 30-50-30 and 30-100-30 NSN. Burst Pressure: The SEPCONs readily burst at pressures under 1 psi when the flow was directed from the backside of the chip through the…

Posted in NRG Tagged with: , , , , ,

NSN SEPCONs

Still trying to reproduce Joe’s large pore material on SEPCONs using NSN stacks.  This post has data from two wafers with 30/50/30 and 30/100/30 NSN.  RTP is 1000C 50C/s for 1min.  Nitride is etched off by placing samples in 50%…

Posted in NRG Tagged with: , , , ,

Update: 30/100/30 OSO, 30/75/30 & 30/100/30 NSN SEPCON

We are trying to reproduce the very small pores Joe created with 30/100/30 OSO and large pores created with 30/100/30 NSN using a SEPCON pattern.  (Joe’s previous post.) We had a problem with several chips releasing from the center of…