Author: Josh Winans
Josh is a postdoc in the McGrath lab working on disruptive membrane technologies.

SEPCON 0.1% SDS pretreatment

After discussions with the gentleman in charge of surface functionalization at INT last week, Jim suggested that I attempt to pretreat our membranes with 0.1% SDS before a filtration.  The hope being that some surfactant left on the surface of…

Posted in NRG

Specialized Susceptors for SSI RTP in URnano

A new user in URnano has used the “old” susceptor for a ~270 C  (I might have the exact number wrong, but it is relatively low temp) to heat In on GaAs.  I don’t think there was ever a good…

Posted in NRG

Fluorosphere wash and measurement with Tecan and Fluorescent microscope

Karl and I have been working to measure separations using SEPCONs with particles ranging in size from 20 nm to 1 µm. We started out naively enough by slightly diluting some flourospheres we found in the refrigerator, putting them in the…

Posted in NRG Tagged with: , ,

550-600 nm diameter pores in 120 nm thick SiN

Wafer # 4369 (PFI 02) was fabricated with pore sizes ranging from ~550 – 600 nm.  Below are two SEM images of the pores, followed by two STEM images.  The pores are all open and very well defined.  The only…

Posted in NRG

SEPCON assembly – written description

Following is a written protocol for SEPCON assembly.  (Here is a link to a video demonstration) Materials required: wafer tweezers, small sample tweezers (preferably plastic), soft foam board from craft store, wafer of sepcon chips, razor blade, plastic enclosure to…

Posted in Protocols (Public)

Video detailing SEPCON assembly

SEPCON assembly

Posted in Protocols (Public)

Posted in Protocols (Public)

SiN-NP in 50 nm SiN

Using a 6″ wafer, we start with 50 nm of RV SiN, then deposit 40 nm a-Si followed by 20 nm of SiO2.  RTP of 1050 C, 100 C/s, 60s.  JP patterned the wafer to make standard SEPCON chips. The…

Posted in NRG Tagged with: , ,

Updated: 25-40-25 nm OSO SEPCONS

We created a 25-40-25 OSO stack with a SEPCON pattern.  RTP at 1050 C 100 C/s 60 s.  The following images show a comparison between the STEM detector and the SEM detector, and then a couple more images at 100…

Posted in NRG Tagged with: , , ,

Pre-spring lab clean! (and o-rings)

Let’s get a blast-from-the-past and go through a bunch of drawers in the lab!  I spoke with Jim and it seems like it might be best to schedule it during next regularly slotted Tuesday NRG mtg.  So let’s plan on…

Posted in NRG