SEPCON 0.1% SDS pretreatment

After discussions with the gentleman in charge of surface functionalization at INT last week, Jim suggested that I attempt to pretreat our membranes with 0.1% SDS before a filtration.  The hope being that some surfactant left on the surface of…

Posted in NRG

MATLAB Installation

Good morning, We received some messages from customer who are having trouble logging into their Matlab account. If you are having trouble accessing Matlab, please see below for your update instructions. If you continue to have Matlab issues, please contact…

Posted in NRG

Attempts in Making PDMS Gaskets in CytoVu Assemblies Play Nicely with PEGylation

This summer I’ll be working on preliminary development of technology that might lead to SiMPore drug discovery assays. The goal is to use SiMPore membranes to create much more efficient and generalized assays, which represents a big opportunity for the…

Posted in NRG

Problems with lab door

Can someone help explain this e-mail? Hey Jim – Just got a call from the locksmith who had a report from security that someone in your lab is tampering with the lock on your lab door…by doing what they’re doing,…

Posted in NRG

Specialized Susceptors for SSI RTP in URnano

A new user in URnano has used the “old” susceptor for a ~270 C  (I might have the exact number wrong, but it is relatively low temp) to heat In on GaAs.  I don’t think there was ever a good…

Posted in NRG

PEG Microarray Solution Dilution and X-linker Concentration Study

Working on the development of PEG microarrays for cell heterogeneity applications. Current work has been accomplished on TPM coated glass coverslips. Transfer to membranes are in progress. Three different x-linker concentrations were tested in a 1:1 mixture of PEG and…

Posted in NRG

Long Term Urea Clearance in 100% Serum

I ran a 30 hour urea clearance with 100% serum through the single slot dialysis device. The now standard protocol was run. The single slot chip was annealed in the RTP for robustness then clamped into the acrylic/PDMS flow fixture.…

Posted in NRG Tagged with: , , , ,

Process Flows

What process flows have I used to create my devices? Standard Cut out gaskets (10 min) Embed Electrode (face down) (3 hrs) Ozone Bottom, Interstitial, Filter and Top channels together (1 hrs, cure overnight) Ozone Bottom Electrode (1 hr, cure…

Posted in NRG

Microscopy on TEM Grids with Kevin Webb @ University of Nottingham

Dr. Webb is very interested in the thin nanomembranes that our group experiments with. To date, he has been trying to get cells to grow on SiN microporous material and image them with a few different types of microscopy (Phase,…

Posted in NRG

Using Alumina Deposition to Modulate Pore Size

The Cambridge Microsystems Savannah 200 atomic layer deposition (ALD) system uses a two-step chemical process that alternates pulses of water vapor and trimethylaluminum (TMA) to build a layer of Al2O3 on a silicon substate. Because of the two-step nature of…

Posted in NRG Tagged with: , , , , ,