Discoloration in Sepcon

We have seen that discoloration of chips is slower in Sepcons and this has been speculated to be because of the separation between the ‘well side’ and the ‘membrane side’ of the chip existing in the Sepcon format. To further…

Posted in NRG Tagged with: , ,

Pore Processing Comparison of W615

In order to support the idea that RTP treatment does not change membrane pore characteristics (as shown by Anant in the rhodamine diffusion study) I processed TEM samples that were not treated, RTPed in Ar, for 5 minutes at 800C,…

Posted in NRG Tagged with: , , ,

HUVEC spreading on pncSi and glass

Following time lapse movies show the spreading of HUVECs on pncSi and glass ( @ 37C, in L15 media supplemented with 10% FBS) over a time period of ~4 hrs. HUVEC spreading on pncSi HUVEC spreading on glass

Posted in NRG Tagged with: ,

Rhodamine diffusion profiles for non-rtp/rtp pncSi

Following images show the diffusion profile of rhodamine across pncSi as observed in the timelapse movies. Looking at the profiles no significant difference is observed between the non RTPed and RTPed samples. Non RTP sample: RTP sample:

Posted in NRG Tagged with: ,

Fibroblasts spreading on glass

I carried out another trial of spreading experiments and following time lapse movies show the spreading of fibroblasts on glass ( @ 37C, in L15 media supplemented with 10% FBS) over a time period of ~7 hrs. Fibroblast spreading on…

Posted in NRG Tagged with: ,

Cell Spreading on pncSi and glass

Spreading of cells (huvec and fibroblasts) on pncSi and glass was observed at ~37 C in L15 media (+ 10% FBS) for ~5 hours. Its observed that the cell spreading is pretty similar on both the substrates and the time…

Posted in NRG Tagged with: , ,

Rhodamine 6G diffusion through RTP treated and non-treated pncSi (w/o pinholes)

Diffusion of rhodamine was observed through pncSi samples from W620. This was done to compare the porosity of the membranes after RTP treatment. From the following movies (real time = 10 mins) it can be seen that there is no…

Posted in NRG Tagged with: ,

Fibroblast spreading on the membrane

Time lapse movie of fibroblast spreading on the nanomembrane was captured over a period of ~ 8 hours. I was having some problem uploading the video here, thus have done so in the NRG knowledge page under the cell culture…

Posted in NRG Tagged with: , ,

HUVEC adhesion update

Couple of HUVEC adhesion trials were carried out and the results were found satisfactory as seen in the charts below.

Posted in NRG Tagged with: , ,

HUVEC growth kinetics with serum free media as control

HUVEC growth was monitored for 4 days on different substrates (glass, plastic and pncSi), this time in media (EGM) with and without serum. Growth in media w/o serum was observed to be much slower than the growth in media with…