Tag: Hemocompatibility studies

f-BSA adsorption pnc-Si

Samples of pnc-Si, 5.5 mm x 5.5 mm, were functionalized at Adarza and incubated with fluorescein conjugated BSA. Wells were formed in PDMS to hole fluid above the samples. Samples were wetted with PBS then f-BSA, 5 mg/mL, was added.…

Posted in NRG Tagged with: , , , ,

Adsorption of F-BSA on PEGylated pnc-Si, PEGylated Glass, Glass

This study was run to test test the efficacy of PEGylation in blocking BSA adsorption. Three surface types were used, glass, PEGylated glass, and PEGylated pnc-SI. The glass was cleaned in Ethyl Alcohol, dried and UV treated, PEGylated glass was…

Posted in NRG Tagged with: , , ,