f-BSA adsorption pnc-Si

Samples of pnc-Si, 5.5 mm x 5.5 mm, were functionalized at Adarza and incubated with fluorescein conjugated BSA. Wells were formed in PDMS to hole fluid above the samples. Samples were wetted with PBS then f-BSA, 5 mg/mL, was added.…

Posted in NRG Tagged with: , , , ,