Author: Karl Reisig

W565 Air Permeability and Burst Pressure

I tested four samples (-1,1); (-1,2); (-1,3); and (-2,4) for air permeability and burst pressure. The first three samples showed no measurable air permeability for three attempts each. The sample from position (-2,4) did have a very small air permeability…

Posted in NRG Tagged with: ,

Desalting with Dialysis Cassettes

One area of use to explore for the membranes is desalting, the removal of salts from solutions (such as those containing proteins). Two dialysis products made my Thermo/Pierce were tested to develop a protocol and test manufacturer’s claims. These products…

Posted in NRG Tagged with: , ,

HUVEC Adhesion with Controls

HUVEC adhesion was measured on glass, tissue culture plastic, and pnc-Si, with poly-lysine coated plastic and teflon coverslips as positive and negative controls. Adhesion on pnc-Si was low, this could be due to cells being lost through broken slits or…

Posted in NRG Tagged with: , ,

Cell Adhesion Testing 6/3-6/4

Two more adhesion tests were run recently, one on Tuesday and one on Wednesday. For both tests cells were imaged after five hours. Fibroblast trial 3 was the first test where the optimal cell density (assuming 100% of cells are…

Posted in NRG Tagged with: , ,

HUVEC and Fibroblast Growth Summary

Thus far three HUVEC and two L13T3 growth tests have been conducted on substrates including glass,pnc-Si, tissue culture plastic, and untreated plastic. Only one test with untreated plastic has been run for each cell type. Cells on Si samples are…

Posted in NRG Tagged with: , ,

Diffusion Stir Cell Update

Mike and I tested the movement of Rhodamine between the two cell channels to prove that the Rhodamine particles do diffuse through the membrane. After inspection in the microscope we saw that the fluorescence from the Rhodamine does transfer from…

Posted in NRG Tagged with: ,

Adhesion Testing: HUVEC and Fibroblasts

Adhesions tests are being performed to see if cellular attachment varies between our material, glass, and plastic. These experiments are motivated by lower initial cell densities observed on pnc-Si in growth tests; we are investigating if the lower initial densities…

Posted in NRG Tagged with: , ,

Fibroblast Growth Take 3

A third fibroblast (L1 3T3, P22) growth test was conducted using glass, untreated and tissue culture treated plastic, and RTPed pnc-Si (W509) as substrates. Cells were grown in DMEM +10% FBS changed every 48 hours. R values are for the…

Posted in NRG Tagged with: ,

W502 and 504 Testing

W502 and 504 were tested for burst pressure and air permeability. Only one sample from W502 was tested for burst pressure (the other broke while setting up and I wanted to conserve samples) with a burst pressure of 4.46 psi.…

Posted in NRG Tagged with: ,

Fibroblast Growth and Associated pnc-Si Discoloration

A second fibroblast (L1 3T3, P21) growth test was conducted on RTP treated samples from W510, tissue culture plastic (polystyrene), and glass cover slips. Fibroblasts were cultured in DMEM with media changed every 48 hours. Cells were imaged using the…

Posted in NRG Tagged with: , , ,