Tag: closed flow system

Cell growth in micovasculature mimetic device

I am trying to grow HUVECs under flow in my device to establish a tight and confluent monolayer for TEER analysis. My device schematic looks like this and the whole setup is as below I tried to use the NPN…

Posted in NRG Tagged with: , , , ,

Microfluidics in Hemodialysis Project

The purpose of the fluidics in our hemodialysis system is to move the sample to and the retentate away from the membranes. The dialysate (permeate, filtrate) will be handled passively in the initial designs and therefore do not require fluidic…

Posted in NRG Tagged with: , ,

The Whitesides Chamber implemented in the McGrath Lab has now successfully generated a steady and linear gradient

Hi all, After nearly a month of troubleshooting the fabrication of Whitesides Chamber we finally have the capability to generate a steady and linear gradient of molecules.  In the presented case, we have generated a gradient of rhodamine 6G (R6G),…

Posted in NRG Tagged with: , , , , , , ,

Materials in contact with media in micropump

The pump’s data sheet (located here) describes the pumps materials as: polyphenylene sulphone (PPSU) polyimide (PI) nitrile butadiene rubber (NBR) It also says that the acceptable particle tolerance is < 50 μm.    This is the info we will need to…

Posted in NRG Tagged with: , ,

15um Bead Flow through Closed Flow Cell

Based on the results obtained yesterday with the closed flow cell we reran another trial today. The closed flow system we tested today was bound using UV Ozone treatment, surprisingly this system created a relatively strong bond despite our resent…

Posted in NRG Tagged with:

No success with UV Ozone Bonding at 100C with High Humidity

Following the advice of Dave and Chris I ran a UV Ozone bonding trial yesterday with the stage temperature set to 100C (instead of the usual 25C). The idea behind the elevated stage temperature is to drive off any water…

Posted in NRG Tagged with: