Tag: Hemodialysis

First 4-Hour HD with 75-nm NPN

I assembled two 2-chip dialyzers using the thicker, 75-nm NPN membrane chips (10 mm long multichannel, 22 mm x 24 mm). The dialyzers were pumped full of IPA, to fill with fewer bubbles, then infused with PBS for at least…

Posted in NRG Tagged with: , , ,

Surface Modification for Hemodialysis

We are continuing to work with the Shestopalov lab on surface modifiation of hemodialysis filters to prevent adhesion and activation. Jim recently presented our status and strategy (PDF) to the Technical Development Fund and was awarded the balance of the award,…

Posted in NRG Tagged with: , , ,

Urea Clearance: First Animal Study Results

BOTTOM LINE: We had great results from the small number of nanoporous membranes used to clear urea from Sprague-Dawley rats. We are clearing Urea better than commercial materials. (see fig) Recap of previous work: First we leaned how to set…

Posted in NRG Tagged with: , ,

Sham Dialysis Study

We performed four hours of sham dialysis, using two non-porous nitride membranes. The set-up is described in an earlier post. Blood samples were taken when the animal was received, after one week of the adenine containing diet, then at 1 hour…

Posted in NRG Tagged with: ,

Small Animal Model Hemodialysis Set-Up

Sprague-Dawley rats will be purchased from Harlan. These pre-manipulated animals will have been catheterized prior to shipment. We will feed them an adenine rich diet to induce uremia, high levels of urea in the blood. Once uremic, a rat will…

Posted in Protocols Tagged with: ,

Review: Blood Purification 2013

In vitro Clearance and Hemocompatibility Assessment of Ultrathin Nanoporous Silicon Membranes for Hemodialysis Applications Using Human Whole Blood Morteza Ahmadi Maud Gorbet John T.W. Yeow Department of Systems Design Engineering and Waterloo Institute for Nanotechnology, University of Waterloo, Waterloo, Ont. , Canada Summary Two…

Posted in NRG Tagged with: ,

Hemo biometrics for various animals

In determining an appropriate animal model for hemodialysis efficacy, several metrics need to be compared to the human vasculature. Blood volume, blood pressure, and heart rate could effect the suitability of these animals to model clinical hemodialysis. Blood volume can…

Posted in Knowledge Tagged with: , ,

Paper Review… Human Nephron Filter: Nissenson(Watts) UCLA