Tag: gold

TEM images of dried gold solutions

For the modeling paper, I had to precisely quantify the distribution of gold nanoparticles in the BBI solutions. To do this, I dried the stock solutions of particles on TEM grids (I don’t know what chips I used, but I seem…

Posted in NRG Tagged with: ,

Using Alumina Deposition to Modulate Pore Size

The Cambridge Microsystems Savannah 200 atomic layer deposition (ALD) system uses a two-step chemical process that alternates pulses of water vapor and trimethylaluminum (TMA) to build a layer of Al2O3 on a silicon substate. Because of the two-step nature of…

Posted in NRG Tagged with: , , , , ,

SEM Images of Barcikowski Samples

With Joe’s help, I was able to take some SEM images of the samples that I performed my previous set of separation experiments on. Sample 1: The obvious aggregation in this sample (exemplified by the ‘victory eagle’ blot in the…

Posted in NRG Tagged with: , , , , , , ,

Barcikowski Collaboration Rotation Project

As a rotation student from the Biophysics depart, I’ll be spending the next six weeks or so helping Dr. Stephan Barcikowski use the nanomembranes to do a number of separations as part of a nanofabrication procedure. Dr. Barcikowski makes extremely…

Posted in NRG Tagged with: , , ,

Pressurized Gold Separations – Part 3

Dan Mendelson performed gold separations using wafer 255 and has shown that this wafer has a cutoff for gold near 25 nm. Below I have plotted the data of filtrate gold concentration as a function of the feed concentration for…

Posted in NRG Tagged with: , ,
0
    0
    Your Cart